Plastic injection molding materials should be selected by application requirements such as load, heat, impact, chemical exposure, dimensional stability, surface finish, flexibility, flame rating, UV exposure and production cost. Common choices include ABS, PC, nylon, PP, PE, POM, PBT, TPE and PMMA.

Many molded part issues start with an unclear material choice. A resin that is easy to mold may not survive heat, load or chemical exposure, while a high-performance resin may increase cost or require design changes. A practical selection guide should connect part function with manufacturability.

Injection molding material selection samples including ABS PC nylon PP POM TPE PMMA molded parts and resin pellets

Common Injection Molding Materials

Oorzaak / materiaal Typisch kenmerk of gebruik Maatregel van de koper of de technische dienst
ABS Housings, covers, consumer and industrial parts Good processability and surface finish
PC Impact-resistant and transparent components Needs drying and stress-aware design
PA6 / PA66 nylon Gears, brackets, wear parts and structural components Check moisture absorption and glass fiber options
PP Living hinges, clips, containers and lightweight parts Good chemical resistance and fatigue behavior
POM / acetaal Precision gears, bushings and sliding parts Good dimensional stability and wear resistance

How to Choose a Plastic for Injection Molding

  • Define the part’s load, temperature, chemical exposure and assembly method.
  • Separate cosmetic requirements from functional requirements.
  • Confirm whether the part needs stiffness, toughness, flexibility or wear resistance.
  • Review shrinkage, moisture absorption and tolerance needs before tooling.
  • Ask whether a prototype material can transition into production molding.

Material Selection by Application

Materiaal / behuizing Belangrijkste punt van zorg Toelichting bij de selectie
Automotive under-hood parts PA66 GF, PBT, PPS Heat, chemical and dimensional stability matter
Electrical housings ABS, PC-ABS, FR PC, PBT Impact and flame rating may be required
Transparent covers PC, PMMA Balance impact strength and clarity
Flexible grips or seals TPE, TPU Hardness, bonding and compression set matter
Wear and sliding parts POM, nylon, PTFE-filled grades Friction, moisture and tolerance must be checked

Buyer RFQ Details for Material Selection

Voor een nuttige beoordeling kunt u het 3D-model of de 2D-tekening, de harssoort of het beoogde materiaal, foto’s van het onderdeel (indien het defect al aanwezig is), informatie over de machine en de matrijs (indien beschikbaar), het verwachte jaarlijkse productievolume, esthetische eisen, kritische afmetingen, de toepassingsomgeving en eventuele inspectienormen toesturen. Nylon Plastic kan het ontwerp, het materiaal en het spuitgietproces beoordelen voordat er wijzigingen in de matrijzen of de productie worden doorgevoerd.

Where Modified Nylon Fits in the Material Decision

Material Direction When It Is a Practical Starting Point Checks Before Release
Unfilled PA Toughness, fatigue, wear, surface quality, or a balanced cost target leads the decision Moisture state, dimensional change, heat, load and chemical exposure
PA-GF20 Moderate stiffness, creep control, and shrinkage reduction are needed without maximum reinforcement Fiber orientation, weld-line strength, surface, tool wear and conditioned dimensions
PA-CF30 Specific stiffness, lower thermal expansion, weight reduction, or a qualified electrical target matters Conductivity, anisotropy, impact, tooling wear, flow direction and exact grade data
PP, HDPE or LDPE The part requirement calls for an unmodified polyolefin route Shrinkage, stiffness, chemical exposure, hinge behavior, color and application fit

Unfilled PA, PA-GF20, and PA-CF30 are the primary modified-nylon directions to compare when a project needs a nylon-based molding solution. PP, HDPE, and LDPE remain general raw-material options and should not be treated as interchangeable with reinforced nylon.

Hoe nylonplastic het project ondersteunt

Nylon Plastic supports material selection and finished plastic-part manufacturing through its plastic injection molding service. For injection molding material selection, the useful review connects the drawing, material, tooling or machining route, inspection state, and production plan before a quote is approved.

  • Translate load, temperature, humidity, chemicals, tolerance, appearance, annual volume, and approvals into a grade requirement.
  • Review custom modified nylon compounds when a standard PA grade misses stiffness, impact, wear, heat, color, or compliance needs.
  • Connect the selected resin to drying, shrinkage, gate and vent design, sampling, COA, moisture, and lot-traceability controls.

Gerelateerde lezen

Plastic injection molding material selection guide with polymer pellets and molded samples

Veelgestelde vragen

Compare detailed PA66 GF30 properties and grade selection across GF15, GF30 and GF60 glass fiber reinforcement levels in our dedicated glass-filled nylon guide.

What are the most common plastic injection molding materials?

Common choices include nylon, ABS, PC, PP, PE, POM, PBT, TPE, and PMMA. The correct material depends on the part requirement, processing route, and qualified grade.

When should I choose unfilled PA for injection molding?

Start with unfilled PA when toughness, fatigue, wear, surface quality, and a balanced cost target matter more than maximum stiffness or minimum shrinkage.

When is PA-GF20 or PA-CF30 appropriate?

PA-GF20 is a practical moderate-reinforcement direction. PA-CF30 is considered for specific stiffness, lower thermal expansion, weight, or qualified electrical requirements. Both require grade-specific validation.

Can prototype material become the production material?

Sometimes, but compare mechanical behavior, moisture, shrinkage, tolerance, appearance, compliance, processing, and cost in the final production route before approval.

Request an Injection Molding Material Review

Send the drawing, service environment, quantity, current resin, critical features, and approval requirements for a material and process comparison.

Vertel ons meer over uw onderdeel

Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Scroll naar boven