Rang Type Smeltpunt Moisture (50% RH) Key Characteristic
PA6 Aliphatic 220 °C 2.7% Toughness, processability
PA66 Aliphatic 260 °C 2.5% Sterkte, hittebestendigheid
PA11 Bio-based 185°C 0.8% Flexibility, low moisture
PA12 Aliphatic 178°C 0.7% Lowest moisture absorption
PA46 Aliphatic 295 °C 3.5% Highest heat resistance
Nylon grade comparison chart
Each nylon grade fills a specific performance niche

PA6: The Versatile Workhorse

PA6 is the most widely used nylon grade, representing approximately 60% of nylon consumption. It offers an excellent balance of strength, toughness, and processability.

Essentiële eigenschappen

  • Tensile strength: 70-85 MPa
  • Excellent impact resistance
  • Good surface finish and colorability
  • Wider processing window than PA66

PA66: The High-Performance Standard

PA66 applications in automotive
PA66 dominates under-hood automotive applications

PA66 offers approximately 10-15% higher strength and stiffness than PA6, with superior heat resistance. It’s the preferred choice for demanding applications.

PA11 and PA12: The Specialty Nylons

PA11 and PA12 are distinguished by their exceptionally low moisture absorption—less than 1% even at saturation. This gives them outstanding dimensional stability.

PA11 and PA12 applications
PA11 and PA12 excel in chemical resistance and dimensional stability

PA46: The High-Temperature Specialist

PA46 (Stanyl) offers the highest heat resistance of any aliphatic nylon, with a melting point of 295°C.

Selection Guide

Vereiste Aanbevolen leerjaar
General purpose, cost-sensitive PA6
High temperature (>120°C) PA66, PA46
Wet/humid environment PA12, PA11
Maximum stiffness PA66-GF30/50

Onze mogelijkheden

Met meer dan 300 CNC machines, produceren we meer dan 10.000 stuks per dag met toleranties zo nauw als ±0,005mm. Wij accepteren MOQ vanaf 1 stuk, met levertijden variërend van 24 uur tot 15 dagen. We supply all major nylon grades. Ontvang binnen 24 uur een offerte.

FAQ

How do you know whether The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More fits a part?

The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More?

Controleer de sterkte, stijfheid, slagvastheid, hittebestendigheid, vochtopname, maatvastheid, wrijving, slijtage en chemische compatibiliteit.

What is the biggest selection risk for The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More?

Het grootste risico is dat men zich baseert op een waarde uit een datasheet zonder rekening te houden met de daadwerkelijke omgeving, de verwerkingsmethode, de geometrie van het onderdeel en het gebruik op lange termijn.

When should The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More be tested before production?

Het wordt aanbevolen om het onderdeel te testen wanneer het wordt blootgesteld aan belasting, hitte, chemicaliën, vocht, strenge toleranties, wettelijke voorschriften of een nieuwe bedrijfsomgeving.

Laten we een oplossing op maat maken

Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.

Gerelateerde lezen

Scroll naar boven