PA6 GF20 | 20% Glasvezelversterkt nylon 6

What is PA6 GF20?

PA6 GF20 is a reinforced engineering plastic where nylon 6 is compounded with 20% glass fibers. It is strategically positioned to bridge the gap between standard and high-performance grades, delivering a significant and cost-effective boost in mechanical properties over PA6 GF15 without fully committing to the stiffness and processing demands of PA6 GF30. It’s the ideal choice when you need “more than GF15 but not quite GF30.”

Why Choose Nylon Plastic’s PA6 GF20?

✅Optimized Performance per Cost: Achieves an excellent balance, offering more strength for your investment compared to lower-filled grades.

✅  Versatile Application Range: Suitable for a wide array of components that require reliable performance under moderate stress and heat.

✅ Proven Processing Reliability: Our formulation ensures consistent flow and molding behavior for predictable production outcomes.

✅ Snelle levering: Betrouwbare toeleveringsketen van prototype tot massaproductie

Categorieën: , Merk:

万翰详情 01

Technische specificaties Tabel:

Eigendom Waarde Testnorm
Glasvezel inhoud 20% (±2%) ISO 1172
Treksterkte 100 – 145 MPa ISO 527
Flexural Modulus 4,200 – 6,500 MPa ISO 178
Slagvastheid (ingekeepte Izod) 11 – 16 kJ/m² ISO 180
Warmteafbuigingstemperatuur (HDT) 165 – 195 °C @ 1.8 MPa ISO 75
Smeltpunt 215 - 230 °C ISO 3146
Vochtabsorptie ~1.7% (23°C/50% RH) ISO 62

 

Vergelijkingstabel materiaalprestaties PA6-serie:

Eigendom PA6 GF15 PA6 GF20 PA6 GF30 PA6 GF33 PA6 GF40 PA6 GF50 PA6 GF60
Glasvezel inhoud 15% 20% 30% 33% 40% 50% 60%
Treksterkte (MPa) ~118 ~125 ~165 ~175 ~185 ~200 ~220
Flexural Modulus (MPa) ~3,800 ~4,500 ~5,218 ~7,000 ~7,500 ~9,000 ~12,000
Ingeslagen Impact (kJ/m²) ~10 ~12 ~12 ~12.5 ~13 ~14 ~14
HDT @1,8MPa (°C) ~160 ~180 ~190 ~195 ~215 ~216 ~220
Profiel High toughness, cost-effective Balance of toughness & strength Best all-around, most widely used Performance upgrade of GF30 Start of high stiffness & heat resist. Metal-like stiffness & strength Ultimate stiffness for extreme cases

 

Key Advantages of PA6 GF20

✅ Enhanced Strength with Good Toughness:

Offers a noticeable improvement in rigidity and strength over GF15, while retaining better impact resistance than higher GF grades.

✅Improved Thermal Capability:

Higher heat deflection temperature provides a greater safety margin for applications in warm environments.

✅ Cost-Effective Performance Upgrade:

An economical step-up material when PA6 GF15 reaches its mechanical limit.

✅ Good Processability:

Maintains relatively good flow compared to GF30 and above, suitable for molding parts with moderate complexity.

 

Industriële toepassingen:

de cruciale rol van spuitgieten in de auto-industrie

PA6GF20 is commonly used in automotive components, interior parts, and other applications that require a good surface finish and fundamental rigidity.

Aansturen van innovatie in verschillende sectoren

Industrie Belangrijkste toepassingen
Automotive Motorkappen, inlaatspruitstukken, structurele steunen, sensorbehuizingen, connectoren.
Ontdek Automobieltoepassingen →
Elektrisch & elektronica Stroomonderbrekers, schakelaars, connectorbehuizingen, isolerende componenten.
Ontdek E&E-oplossingen →
Industriële apparatuur Tandwielen, lagers, machinebehuizingen, rollen, mechanische onderdelen.
Zie Industrieel gebruik →
Verschillende toepassingsscenario's van PA-kunststoffen
Verschillende toepassingsscenario's van PA-kunststoffen

Hoe kiezen?

Eenvoudig gezegd:

  • Voor goede taaiheid of kosteneffectiviteit, overweeg PA6 GF15.

  • Voor evenwichtige algemene prestaties, kiezen PA6 GF30.

  • Voor hogere stijfheid, sterkte en hittebestendigheid, en als de kosten minder gevoelig zijn, overweeg dan PA6 GF40/50/60. Over het algemeen verbetert een hoger glasvezelgehalte deze eigenschappen.

Waarom voor ons kiezen?

万翰详情 03

万翰详情 04

FAQ Sectie:

V: Kan ik een monster krijgen voordat ik een bestelling plaats?
A: Ja! We leveren gratis monsters voor gekwalificeerde projecten.

V: Wat is de productietijd?
A: Standaardkwaliteiten: 5-7 dagen; aangepaste formuleringen: 2-3 weken.

V: Leveren jullie materiaalcertificaten?
A: Ja, we leveren volledige materiaaldocumentatie en certificeringen.

Tell Us About Your Part

Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Scroll naar boven

Neem contact op

Vul het onderstaande formulier in en we nemen binnenkort contact met u op.

Contactgegevens