PA66 GF25 Glass Fiber Reinforced Nylon 66 Pellets

PA66 GF25 is nylon 66 reinforced with 25% glass fiber, supplied in pellet form. PA66 WHG25A is the reference formulation on this page. Review it for reinforced covers, fan components and mounting parts with defined heat, load and moisture requirements.

Reference grade: PA66 WHG25A

Supply: 25% glass fiber reinforced pellets. Confirm color, quantity and required documents with your inquiry.

Categorieën: ,

PA66 GF25 Material Overview

PA66 GF25 is nylon 66 reinforced with 25% glass fiber, supplied in pellet form. PA66 WHG25A is the reference formulation on this page. Review it for reinforced covers, fan components and mounting parts with defined heat, load and moisture requirements.

Item Details
Reference grade PA66 WHG25A
Polymer PA66 (nylon 66)
Versterking 25% glass fiber
Formulier Pellets for material-supply inquiries
Color and processing Confirm the offered grade and current processing guidance

Reference Material Properties

Typical values for PA66 WHG25A from the linked supplier PDF.

Eigendom Typische waarde Testmethode
Treksterkte 155 MPa ISO 527-2
Tensile strain at break 10% ISO 527-2
Buigmodulus 5820 MPa ISO 178
Deflection temperature under load 210 °C ISO 75-2/B
Dichtheid 1.33 g/cm³ ISO 1183

Specimen conditioning is not stated in the reference sheet. These values are not guaranteed specification limits. Only rows with a usable property, unit and method are reproduced; request clarification of the remaining sheet entries before relying on them for design.

Download PA66 WHG25A supplier reference datasheet (PDF)

Application Review

PA66 GF25 illustrative component applications
Illustrative component concepts. Confirm the selected formulation for the actual part.

Reinforced equipment covers

Define sealing faces, mounting bosses and dimensional references. Validate fit after the specified moisture and temperature conditioning.

Fan components

Review blade roots, mounting points and operating clearance. Part tests should reflect the speed, temperature and vibration of the assembly.

Loaded mounting parts

Check fastener loads, creep and service-fluid exposure. Qualify the material and component together when replacing an existing resin.

Processing and Part Checks

Follow WHG25A drying and molding guidance. Review gate and weld-line placement, fastener regions and dimensional change after conditioning. Heat-deflection data should not be treated as a continuous service-temperature rating.

For component production, review our spuitgietdienst. For other resin options, browse engineering plastic materials.

Material Supply and Manufacturing Support

Nylon Kunststof connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.

Material feeding equipment at WANHAN, Nylon Plastic’s cooperating factory
Material feeding
Extruded plastic strands at the WANHAN cooperating factory
Extrusion process
Laboratory work area at the WANHAN cooperating factory
Laboratory

Grade and formulation selection

Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.

Quality documents for your order

Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.

Support beyond resin pellets

For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.

Cooperating Factory Management-System Certificates

The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.

Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.

Veelgestelde vragen

What material does this page cover?

PA66 GF25 is nylon 66 reinforced with 25% glass fiber, supplied in pellet form. PA66 WHG25A is the reference formulation on this page. Review it for reinforced covers, fan components and mounting parts with defined heat, load and moisture requirements.

Does the 210 °C deflection result define continuous use temperature?

No. The PDF lists a deflection-under-load result under ISO 75-2/B. Long-term temperature capability depends on time, load, moisture and the actual component; it needs separate evidence.

Are these values a production specification?

No. They are typical reference values for PA66 WHG25A. Agree the current grade, test conditions, acceptance limits and required documents for the order.

Do the images show the exact supplied color and finished parts?

The images illustrate resin appearance and possible component concepts. Confirm color and finish on the offered material and samples; the pictured parts do not establish suitability for your design.

What is required for a material replacement?

Identify the current resin and reason for changing it. Compare exact-grade data, dimensions, loads, temperature and environmental exposure, then validate the intended part before production.

What should I send for a quote or sample request?

Send the reference grade, application, color, estimated material quantity and required documents. For a molded-part inquiry, add the drawing, critical dimensions and acceptance requirements. A CAD file is optional for a material-only inquiry.

Related Material Grades

PA66 GF20   |   PA66 GF30

Request Material Data and a Quote

Share the grade, application, service conditions, color, quantity and required documents so the offered material can be reviewed against your project.

Request PA66 WHG25A TDS and Quote

Scroll naar boven

Neem contact op

Vul het onderstaande formulier in en we nemen binnenkort contact met u op.

Contactgegevens