Vochtabsorptie

Toestand PA6 PA66
50% RH 2.7% 2.5%
Verzadiging 8-10% 6-8%

Effects

  • Reduces strength and stiffness
  • Increases impact resistance
  • Changes dimensions

Drying Guidelines

  • PA6: 80°C for 4-6 hours
  • PA66: 100°C for 4-6 hours

FAQ

How do you know whether Moisture Effects on Nylon — Storage & Drying Guide fits a part?

Moisture Effects on Nylon — Storage & Drying Guide fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Moisture Effects on Nylon — Storage & Drying Guide?

Controleer de sterkte, stijfheid, slagvastheid, hittebestendigheid, vochtopname, maatvastheid, wrijving, slijtage en chemische compatibiliteit.

What is the biggest selection risk for Moisture Effects on Nylon — Storage & Drying Guide?

Het grootste risico is dat men zich baseert op een waarde uit een datasheet zonder rekening te houden met de daadwerkelijke omgeving, de verwerkingsmethode, de geometrie van het onderdeel en het gebruik op lange termijn.

When should Moisture Effects on Nylon — Storage & Drying Guide be tested before production?

Het wordt aanbevolen om het onderdeel te testen wanneer het wordt blootgesteld aan belasting, hitte, chemicaliën, vocht, strenge toleranties, wettelijke voorschriften of een nieuwe bedrijfsomgeving.

Vertel ons meer over uw onderdeel

Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.

Gerelateerde lezen

Scroll naar boven