PA66 GF25 Material Overview
PA66 GF25 is nylon 66 reinforced with 25% glass fiber, supplied in pellet form. PA66 WHG25A is the reference formulation on this page. Review it for reinforced covers, fan components and mounting parts with defined heat, load and moisture requirements.
| Item | Details |
|---|---|
| Reference grade | PA66 WHG25A |
| Polymer | PA66 (nylon 66) |
| Versterking | 25% glass fiber |
| Formulier | Pellets for material-supply inquiries |
| Color and processing | Confirm the offered grade and current processing guidance |
Reference Material Properties
Typical values for PA66 WHG25A from the linked supplier PDF.
| Eigendom | Typische waarde | Testmethode |
|---|---|---|
| Treksterkte | 155 MPa | ISO 527-2 |
| Tensile strain at break | 10% | ISO 527-2 |
| Buigmodulus | 5820 MPa | ISO 178 |
| Deflection temperature under load | 210 °C | ISO 75-2/B |
| Dichtheid | 1.33 g/cm³ | ISO 1183 |
Specimen conditioning is not stated in the reference sheet. These values are not guaranteed specification limits. Only rows with a usable property, unit and method are reproduced; request clarification of the remaining sheet entries before relying on them for design.
Application Review

Reinforced equipment covers
Define sealing faces, mounting bosses and dimensional references. Validate fit after the specified moisture and temperature conditioning.
Fan components
Review blade roots, mounting points and operating clearance. Part tests should reflect the speed, temperature and vibration of the assembly.
Loaded mounting parts
Check fastener loads, creep and service-fluid exposure. Qualify the material and component together when replacing an existing resin.
Processing and Part Checks
Follow WHG25A drying and molding guidance. Review gate and weld-line placement, fastener regions and dimensional change after conditioning. Heat-deflection data should not be treated as a continuous service-temperature rating.
For component production, review our spuitgietdienst. For other resin options, browse engineering plastic materials.
Material Supply and Manufacturing Support
Nylon Kunststof connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.



Grade and formulation selection
Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.
Quality documents for your order
Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.
Support beyond resin pellets
For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.
Cooperating Factory Management-System Certificates
The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.
Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.
Veelgestelde vragen
What material does this page cover?
PA66 GF25 is nylon 66 reinforced with 25% glass fiber, supplied in pellet form. PA66 WHG25A is the reference formulation on this page. Review it for reinforced covers, fan components and mounting parts with defined heat, load and moisture requirements.
Does the 210 °C deflection result define continuous use temperature?
No. The PDF lists a deflection-under-load result under ISO 75-2/B. Long-term temperature capability depends on time, load, moisture and the actual component; it needs separate evidence.
Are these values a production specification?
No. They are typical reference values for PA66 WHG25A. Agree the current grade, test conditions, acceptance limits and required documents for the order.
Do the images show the exact supplied color and finished parts?
The images illustrate resin appearance and possible component concepts. Confirm color and finish on the offered material and samples; the pictured parts do not establish suitability for your design.
What is required for a material replacement?
Identify the current resin and reason for changing it. Compare exact-grade data, dimensions, loads, temperature and environmental exposure, then validate the intended part before production.
What should I send for a quote or sample request?
Send the reference grade, application, color, estimated material quantity and required documents. For a molded-part inquiry, add the drawing, critical dimensions and acceptance requirements. A CAD file is optional for a material-only inquiry.
Related Material Grades
Request Material Data and a Quote
Share the grade, application, service conditions, color, quantity and required documents so the offered material can be reviewed against your project.